Matsayi na EU Rohs 2.0 Buƙatar abun ciki (PB) ba ta wuce 1000ppmu ba kamar yadda C17300.Kou ya inganta jan ƙarfe na C17300.bou ya samar da jan karfe na C17300 . Ayyukan yankan wannan C17200 yana da kyau.

1

Abin ƙwatanci

Be

Ni + co

Ni + co + fe

Pb

Cu

C17300

1.8-2

≥0.20

≤0.6

<0.1

Sakewa

2. Kayan aiki da kayan aikinlow jagorantaC17300

Jiha
(A cewar Ashm)

Jiyya zafi
(℃)

Diamita

(mm)

Tenerile ƙarfi (MPa)

Yawan amfanin ƙasa (MPA)

Elongation

4xd (%)

Ƙanƙanci

Aikin lantarki

(IAacs,%)

HV0.5

Hrb ko hrc

Tb00

775 ℃ ~ 800 ℃

Duka

410-590

> 140

> 20

159-162

B45-B85

15-19

Td04

775 ℃ ~ 800 ℃ bayani + Tsari Tsara Hardening

8-20

620-860

> 520

> 8

175-257

B88-B102

15-19

0.6-8

620-900

> 520

> 8

175-260

B88-B103

Th04

315 ℃ x1 ~ 2hr

8-20

1140-1380

> 930

> 20

345-406

C27-C44

23-28

0.6-8

1210-1450

> 1000

> 4

35415

C38-C45